Bul.23-ti Pehoten Shipchenski Polk No:114 Kazanlak/Bulgaria
EN
BG
Search for:
(Product Name, AWS or EN Norm)
Search product
EMAIL US
info@weld-inn.com
Home
Products
About
Contact
WI 350 G
Home
Products
Weld-inn Welding Consumables
Weld-inn Welding Wires
Weld-inn Hardfacing Welding Wire
WI 350 G
Brand
Weld-inn
Product
WI 350 G
Datasheet
Standards
DIN 8555
MSG 5-GZ-350
Chemical Composition of Weld Metal % (Typical)
C
Mn
Si
Cr
Mo
0.50
0.90
0.55
6.00
0.90
Mechanical Properties
Hardness (after working) (HRC)
36 - 40
Features and Applications
Cr-Mo alloyed steels (2.5%-1.0%) resistant to high temperature, wear, pressure and shocks
Good resistance to cracking and to the attack of sulphures agents
Guide rollers, excavators, screw conveyers, gears, moulds, rolling surfaces, etc
Before the application of welding , it is recommended pre-heating of 200°C
lf necessary , post- weld stress relief should be made at 660°C
Shielding Gas: Ar+CO2 mix gases can be used
Current Type
MAG D.C.(+)
Welding Positions
Operating Data
Product code
Package Type
Weight (Kg)
Diameter x Length (mm) / (inch)
1011100195
BS 300 Spool
15
1.20 // 0.047”